Material Notes:
Information provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Water Absorption 0.17 %
0.17 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 218 MPa
31600 psi
Elongation at Break 1.6 %
1.6 %
Flexural Strength 297 MPa
43100 psi
Flexural Modulus 17.8 GPa
2580 ksi
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
Izod Impact, Unnotched (ISO) 43.2 kJ/m²
20.6 ft-lb/in²
Electrical Properties Metric English Comments
Volume Resistivity 5500 ohm-cm
5500 ohm-cm