Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: High Loaded SealsCertified for use in potable water and/or in foodstuffInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
Open Porosity <= 2.5 %
<= 2.5 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
Size/Load - 5/100
Hardness, Shore C 100
100
Modulus of Elasticity 26.9 GPa
3900 ksi
Flexural Strength 75.8 MPa
11000 psi
Compressive Strength 200 MPa
29000 psi
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 °C
2.50 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 13.8 W/m-K
96.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
In oxygen
Maximum Service Temperature, Inert 260 °C
500 °F
Reducing Atm.
Descriptive Properties Value Comments
Impregnation Resin
Users viewing this material also viewed the following: