Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: High Loaded SealsCertified for use in potable water and/or in foodstuffInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
Open Porosity 11 %
11 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
Size/Load - 5/100
Hardness, Shore C 83
83
Modulus of Elasticity 22.1 GPa
3200 ksi
Flexural Strength 55.2 MPa
8000 psi
Compressive Strength 155 MPa
22500 psi
Thermal Properties Metric English Comments
CTE, linear 3.06 µm/m-°C

@Temperature 20.0 °C
1.70 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 12.1 W/m-K
84.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 399 °C
750 °F
In oxygen
Maximum Service Temperature, Inert 1204 °C
2199 °F
Reducing Atm.