SGL Carbon Group EK 17 Carbon Graphite

Category Carbon , Graphite
Manufacturer SGL Carbon Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SGL Carbon Group EK 17 Carbon Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: Gliding elementsInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
Open Porosity 5.0 %
5.0 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
Size/Load - 10/100
Modulus of Elasticity 30.3 GPa
4400 ksi
Flexural Strength 68.9 MPa
10000 psi
Compressive Strength 148 MPa
21500 psi
Thermal Properties Metric English Comments
CTE, linear 1.98 µm/m-°C

@Temperature 20.0 °C
1.10 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 399 °C
750 °F
In oxygen
Maximum Service Temperature, Inert 1204 °C
2199 °F
Reducing Atm.