S&E Specialty Polymers TufTech™ XP-116-221(1) PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ XP-116-221(1) PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Automotive – PVC, integral colored, exterior weatherable, extrusion & injection molding compoundInformation provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792, A
Mechanical Properties Metric English Comments
Hardness, Shore A 70.0

@Time 15.0 sec
70.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 12.0 MPa
1740 psi
Type IV 500mm/min; ASTM D638
Elongation at Break 300 %
300 %
Type IV 500mm/min; ASTM D638