S&E Specialty Polymers TufTech™ GM-3958-095 PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ GM-3958-095 PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: A clear, non-toxic, extrusion compound for food contact use.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 58.0
58.0
ASTM D2240
Tensile Strength 10.3 MPa
1490 psi
ASTM D412
Elongation at Break 380 %
380 %
ASTM D412
Processing Properties Metric English Comments
Processing Temperature 166 - 171 °C
330 - 340 °F
Suggested Stock