Material Notes:
Application: An 80°C rated, PVC based, highly flame retardant jacketing compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 89.0

@Time 15.0 sec
89.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 17.9 MPa
2600 psi
ASTM D412
Elongation at Break 250 %
250 %
ASTM D412
Thermal Properties Metric English Comments
Oxygen Index 43.0 %
43.0 %
ASTM D2863