S&E Specialty Polymers TufTech™ 5501124 Vinyl

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ 5501124 Vinyl.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Replacement for TPV/TPR materials for application requiring an excellent compression set properties, Weatherable, Elastomeric, Extrusion Molding Compound. Targeting for GMP PVC 088.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 55.0

@Time 15.0 sec
55.0

@Time 0.00417 hour
ISO 868
Tensile Strength at Break 7.72 MPa
1120 psi
Elongation at Break 450 %
450 %
500mm/min; ISO 257, 1A
Tear Strength 10.4 kN/m
59.3 pli
Method B, angle die, 500mm/min.; ISO 34-1
Compression Set 15.0 %

@Temperature 24.0 °C,
Time 86400 sec
15.0 %

@Temperature 75.2 °F,
Time 24.0 hour
ISO 815-1, Type A
35.0 %

@Temperature 70.0 °C,
Time 79200 sec
35.0 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815-1, Type A
35.0 %

@Temperature 100 °C,
Time 252000 sec
35.0 %

@Temperature 212 °F,
Time 70.0 hour
ISO 815-1, Type A
Descriptive Properties Value Comments
Cold Flex -34°C
SAE J323, Method A, No cracks, 6 mm mandrel