S&E Specialty Polymers GR-1409 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GR-1409 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: High flow, high impact rigid PVC based compound. It is suitable for injection molding of the large parts.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.33 g/cc
1.27 - 1.33 g/cc
ASTM D792
Melt Flow 7.0 g/10 min

@Load 20.0 kg,
Temperature 190 °C
7.0 g/10 min

@Load 44.1 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ASTM D2240
Tensile Strength >= 41.4 MPa
>= 6000 psi
ASTM D638
Flexural Modulus >= 2.76 GPa
>= 400 ksi
ASTM D790
Izod Impact, Notched >= 6.94 J/cm

@Thickness 3.17 mm
>= 13.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Descriptive Properties Value Comments
Falling Weight >2 in-lb/mil
73°F @ 0.125", ASTM D4226
Users viewing this material also viewed the following: