Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers GPP1001V0M-HCO-15 PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer S&E Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GPP1001V0M-HCO-15 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A medium flow polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high level of flame retardancy.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.960 - 1.00 g/cc
0.960 - 1.00 g/cc
ASTM D1505
Melt Flow 12 - 18 g/10 min
12 - 18 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 18.6 MPa
>= 2700 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Modulus >= 0.931 GPa
>= 135 ksi
ASTM D790-79
Izod Impact, Notched >= 0.400 J/cm
>= 0.750 ft-lb/in
ASTM D256
Dart Drop, Total Energy >= 20.3 J
>= 15.0 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Flammability Test 5.0
5.0
Oxygen Index >= 28 %
>= 28 %
ASTM D2863
Users viewing this material also viewed the following: