Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers GPP1001M-P-2986 Grey PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GPP1001M-P-2986 Grey PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: High impact resistance, non-blooming flame retardant polypropylene compound for UL94-V0 injection molding applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.920 - 1.02 g/cc
0.920 - 1.02 g/cc
ASTM D792
Melt Flow 15 - 21 g/10 min
15 - 21 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 10.3 MPa
>= 1500 psi
ASTM D638
Tensile Strength, Yield >= 25.5 MPa
>= 3700 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Modulus >= 1.38 GPa
>= 200 ksi
ASTM D790
Izod Impact, Notched >= 0.641 J/cm
>= 1.20 ft-lb/in
ASTM D256
Gardner Impact >= 16.3 J
>= 12.0 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Flammability Test 5.0

@Thickness 1.59 mm
5.0

@Thickness 0.0625 in
Oxygen Index >= 28 %
>= 28 %
ASTM D2863