Material Notes:
Description: Matte finish, expandable oil resistant flexible PVC/Nitrile alloyInformation provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 69
60 - 69
ASTM D2240
Tensile Strength 10.9 MPa
1580 psi
ASTM D412
Elongation at Break 430 %
430 %
ASTM D412