Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GA-3133S-CCUV PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Meets style 1277 T.C. Power & Control Cable Requirements and can be used for CM(X), CATV(X) and CL2 jacketing applications. UL listed for 720hr. sunlightInformation provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.40 - 1.44 g/cc
1.40 - 1.44 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 92 - 95
92 - 95
ASTM D2240
Tensile Strength 19.3 MPa
2800 psi
ASTM D412
19.88 MPa

@Treatment Temp. 100 °C,
Time 605000 sec
2883 psi

@Treatment Temp. 212 °F,
Time 168 hour
Oven aged
Elongation at Break 280 %
280 %
ASTM D412
238 %

@Treatment Temp. 100 °C,
Time 605000 sec
238 %

@Treatment Temp. 212 °F,
Time 168 hour
Oven aged
Thermal Properties Metric English Comments
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
Oxygen Index 29 %
29 %
ASTM D2863