Material Notes:
Application: 105° C PVC insulating compound designed for SJEOO applicationsInformation provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 84
75 - 84
ASTM D2240
Tensile Strength 18.3 MPa
2650 psi
ASTM D412
15.55 MPa

@Treatment Temp. 60.0 °C,
Time 605000 sec
2255 psi

@Treatment Temp. 140 °F,
Time 168 hour
Oil oven aged
15.74 MPa

@Treatment Temp. 136 °C,
Time 605000 sec
2283 psi

@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
Elongation at Break 350 %
350 %
ASTM D412
329 %

@Treatment Temp. 60.0 °C,
Time 605000 sec
329 %

@Treatment Temp. 140 °F,
Time 168 hour
Oil oven aged
332.5 %

@Treatment Temp. 136 °C,
Time 605000 sec
332.5 %

@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
100% Modulus 0.00965 GPa
1.40 ksi
ASTM D412
Thermal Properties Metric English Comments
Oxygen Index 27 %
27 %
ASTM D2863