Material Notes:
Application: General purpose PVC material with good low temperature properties designed for T-Molding extrusion applicationsInformation provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.33 g/cc
1.27 - 1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 90
85 - 90
ASTM D2240
Tensile Strength 16.2 MPa
2350 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D412
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D412