SCG Chemicals EL-Leneâ„¢ H5480S High Density Polyethylene Monofilament

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , HDPE, Fiber Grade
Manufacturer SCG Chemicals Co.
Trade Name EL-Lene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Leneâ„¢ H5480S High Density Polyethylene Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Characteristics:High tenacityExcellent product colorRecommended Applications: Monofilament and flat yarn extrusion for manufacturing of nets, ropes and tarpaulinInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.954 g/cc
0.954 g/cc
ASTM D1505
Environmental Stress Crack Resistance 30 hour

@Temperature 50.0 °C
30 hour

@Temperature 122 °F
F50, 25% Igepal; ASTM D1693
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength at Break 26.0 MPa
3770 psi
ASTM D638
Tensile Strength, Yield 38.2 MPa
5550 psi
ASTM D638
Elongation at Break 1200 %
1200 %
ASTM D638
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Izod Impact, Notched >= 1.37 J/cm

@Temperature 0.000 °C
>= 2.57 ft-lb/in

@Temperature 32.0 °F
ASTM D256
>= 1.67 J/cm

@Temperature 23.0 °C
>= 3.12 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 131 °C
268 °F
ASTM D2117
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746