SABIC PP 510P Polypropylene Homopolymer for Fiber Applications

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer SABIC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC PP 510P Polypropylene Homopolymer for Fiber Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: PP 510P is a homopolymer specially designed for fiber extrusion applications with the following features:Consistent processabilityGood thread line stabilityGood color consistencyGood gas fading resistanceTypical Applications: PP 510P can be used for medium spin equipment for producing staple fiber of 6 dtex and higher. It can also be used for the production of continuous filament for stitching yarn.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus, 1% Secant 1530 MPa
222000 psi
ASTM D790A
Izod Impact, Notched 0.220 J/cm
0.412 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648
Vicat Softening Point 153 °C
307 °F
ASTM D1525B
Processing Properties Metric English Comments
Processing Temperature 210 - 240 °C
410 - 464 °F
Barrel Temperature