Material Notes:
Product Description: P5510 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applications. It provides excellent stress crack resistance properties combined with very good long term hydrostatic strength.Typical Applications: Pressure pipes for drinking water, irrigation, gas distribution and waste water pipes. It is also recommended for the manufacture of chemical liners and containers.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ISO 1183
Oxidative Induction Time (OIT) >= 20 min

@Temperature 210 °C
>= 20 min

@Temperature 410 °F
EN 728
Carbon Black Loading 2.25 %
2.25 %
ISO 6964
Melt Flow 0.43 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.43 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
10.3 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10.3 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ISO 868
Tensile Strength, Yield 22.0 MPa

@Thickness 2.00 mm
3190 psi

@Thickness 0.0787 in
ISO 527-2
Elongation at Yield 8.0 %

@Thickness 2.00 mm
8.0 %

@Thickness 0.0787 in
ISO 527-2
Tensile Modulus 0.850 GPa

@Thickness 2.00 mm
123 ksi

@Thickness 0.0787 in
ISO 527-2
Charpy Impact, Notched 0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179
2.40 J/cm²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 70.0 °C

@Load 5.10 kg
158 °F

@Load 11.2 lb
ISO 306
Processing Properties Metric English Comments
Melt Temperature 190 - 220 °C
374 - 428 °F