Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Xenoy® 1760 PBT+PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Xenoy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Xenoy® 1760 PBT+PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 84.0 MPa
12200 psi
SABIC - Japan Method
Elongation at Break 11 %
11 %
SABIC - Japan Method
Flexural Strength 127 MPa
18400 psi
ASTM D790
Flexural Modulus 3.92 GPa
569 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C

@Thickness 3.20 mm
244 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C

@Thickness 3.20 mm
257 °F

@Thickness 0.126 in
unannealed; ASTM D648
Copyright © lookpolymers.com All Rights Reserved