SABIC Innovative Plastics Valox® VIC4350 PBT (Asia Pacific)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Valox®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Valox® VIC4350 PBT (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0010 - 0.0030 in/in

@Thickness 0.126 in
SABIC Method
0.0070 - 0.0090 cm/cm

@Thickness 6.40 mm
0.0070 - 0.0090 in/in

@Thickness 0.252 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 106 MPa
15400 psi
SABIC - Japan Method
Elongation at Break 5.0 %
5.0 %
SABIC - Japan Method
Flexural Strength 169 MPa
24500 psi
ASTM D790
Flexural Modulus 8.33 GPa
1210 ksi
ASTM D790
Izod Impact, Notched 1.37 J/cm
2.57 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 206 °C

@Thickness 3.20 mm
403 °F

@Thickness 0.126 in
unannealed; ASTM D648