Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Valox® VAC3001 PBT (Asia Pacific)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Valox®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Valox® VAC3001 PBT (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D 792
Water Absorption 0.080 %

@Time 86400 sec
0.080 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.017 - 0.023 cm/cm

@Thickness 3.20 mm
0.017 - 0.023 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D 785
Tensile Strength, Yield 51.0 MPa
7400 psi
SABIC - Japan Method
Elongation at Break 160 %
160 %
SABIC - Japan Method
Flexural Strength 84.0 MPa
12200 psi
ASTM D 790
Flexural Modulus 2.30 GPa
334 ksi
ASTM D 790
Izod Impact, Notched 0.590 J/cm

@Temperature 23.0 °C
1.11 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature -30.0 - 30.0 °C
72.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C

@Thickness 3.20 mm
131 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D 257
Dielectric Constant 3.3

@Frequency 50.0 - 60.0 Hz
3.3

@Frequency 50.0 - 60.0 Hz
ASTM D 150