Material Notes:
Environmentally sustainable Valox iQ* PBT-ionomer resin for the fibers market. Available in natural color (1001) for use in extrusion/compounding operations. This resin is primarily used as an additive for nylon fibers to enhance cationic dyeability.
Physical Properties Metric English Comments
Viscosity Measurement 0.42 - 0.52
0.42 - 0.52
Intrinsic Viscosity [dl/g]; SABIC Method
Chemical Properties Metric English Comments
Acid Value 50 - 180
50 - 180
meq/kg; SABIC Method
Users viewing this material also viewed the following: