SABIC Innovative Plastics ULTEM JD7101 PEI (Asia Pacific)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics ULTEM JD7101 PEI (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 127 MPa
18400 psi
SABIC - Japan Method
Elongation at Break 6.0 %
6.0 %
SABIC - Japan Method
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 5.09 GPa
738 ksi
ASTM D790
Izod Impact, Notched 0.440 J/cm
0.824 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 208 °C

@Thickness 3.20 mm
406 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 10000 - 1.00e+6 ohm
10000 - 1.00e+6 ohm
ASTM D257