Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI) + PCE
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics ULTEM ATX200 PEI+PCE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 24 g/10 min

@Load 6.60 kg,
Temperature 337 °C
24 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 96.0 MPa
13900 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 70 %
70 %
Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 144 MPa
20900 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 3.17 GPa
460 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
21.36 J/cm

@Thickness 3.20 mm
40.02 ft-lb/in

@Thickness 0.126 in
ASTM D256
Izod Impact, Unnotched 20.82 J/cm
39.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 190 °C

@Thickness 6.40 mm
374 °F

@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 115 °C
239 °F
UL 746B
UL RTI, Mechanical with Impact 115 °C
239 °F
UL 746B
UL RTI, Mechanical without Impact 115 °C
239 °F
UL 746B
Flammability, UL94 V-2

@Thickness 0.760 mm
V-2

@Thickness 0.0299 in
UL 94
V-0

@Thickness 1.49 mm
V-0

@Thickness 0.0587 in
UL 94
Electrical Properties Metric English Comments
Comparative Tracking Index 100 - 175 V
100 - 175 V
UL 746A
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
0.00 - 15 arcs
UL 746A