SABIC Innovative Plastics ULTEM 9075 PEI (Asia Pacific)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics ULTEM 9075 PEI (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Halogen Content 0.00 %
0.00 %
SABIC Method
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 2.4 g/10 min

@Load 6.60 kg,
Temperature 295 °C
2.4 g/10 min

@Load 14.6 lb,
Temperature 563 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 96.0 MPa
13900 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 85 %
85 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 3.30 GPa
479 ksi
5 mm/min; ASTM D638
Flexural Strength 141 MPa
20500 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Yield Strength 144 MPa
20900 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 3.24 GPa
470 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
20.82 J/cm

@Thickness 3.20 mm
39.00 ft-lb/in

@Thickness 0.126 in
ASTM D256
Gardner Impact 35.0 J
25.8 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 188 °C

@Thickness 6.40 mm
370 °F

@Thickness 0.252 in
unannealed; ASTM D648
Descriptive Properties Value Comments
FAA Flammability, FAR 25.853 A/B SECT A-1
FAR 25.853
OSU total heat release (2 minute test) 10kW-min/m^2
FAR 25.853
Vertical Burn a (60s) passes at 1sec
FAR 25.853
Vertical Burn b (12s) passes at 0sec
FAR 25.853