Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility information and should not be used for medical applications which require biocompatibility. Alternative grade HU2400.
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ISO 1183
Moisture Absorption 0.400 %
0.400 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.80 %
0.80 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
on Tensile Bar; SABIC Method
Melt Index of Compound 5.0 g/10 min

@Load 5.00 kg,
Temperature 360 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 680 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 170 MPa
24700 psi
ISO 2039-1
Tensile Strength at Break 180 MPa
26100 psi
5 mm/min; ISO 527
Elongation at Break 2.0 %
2.0 %
5 mm/min; ISO 527
Tensile Modulus 11.5 GPa
1670 ksi
1 mm/min; ISO 527
Flexural Strength 240 MPa
34800 psi
2 mm/min; ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
35.0 kJ/m²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Taber Abrasion, mg/1000 Cycles 20
20
CS-17, 1 kg; SABIC Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.33 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow 45.0 µm/m-°C

@Temperature 23.0 - 150 °C
25.0 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
Thermal Conductivity 0.330 W/m-K
2.29 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 217 °C
423 °F
Rate B/50; ISO 306
225 °C
437 °F
Rate B/120; ISO 306
230 °C
446 °F
Rate A/50; ISO 306
Glass Transition Temp, Tg 217 °C
423 °F
Oxygen Index 48 %
48 %
ISO 4589
Glow Wire Test 960 °C

@Thickness 3.20 mm
1760 °F

@Thickness 0.126 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 3.1

@Frequency 1.00e+6 Hz
3.1

@Frequency 1.00e+6 Hz
IEC 60250
3.5

@Frequency 50.0 - 60.0 Hz
3.5

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 16.0 kV/mm

@Thickness 3.20 mm
406 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
26.0 kV/mm

@Thickness 1.60 mm
660 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
35.0 kV/mm

@Thickness 0.800 mm
889 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
Dissipation Factor 0.0019

@Frequency 1.00e+6 Hz
0.0019

@Frequency 1.00e+6 Hz
IEC 60250
0.0025

@Frequency 50.0 - 60.0 Hz
0.0025

@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index >= 100 V
>= 100 V
IEC 60112
150 V
150 V
IEC 60112
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2
Copyright © lookpolymers.com All Rights Reserved