Material Notes:
SABIC® STAMAX 20YK270 is a 20% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 80929423.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Filler Content 20 %
20 %
glass; ISO 3451
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
50 mm/min, 1A; ISO 527
40.0 MPa

@Temperature 120 °C
5800 psi

@Temperature 248 °F
50 mm/min, 1A; ISO 527
54.0 MPa

@Temperature 80.0 °C
7830 psi

@Temperature 176 °F
50 mm/min, 1A; ISO 527
Elongation at Break 2.4 %
2.4 %
50 mm/min; ISO 527
Tensile Modulus 4.45 GPa
645 ksi
1 mm/min; ISO 527
2.85 GPa

@Temperature 120 °C
413 ksi

@Temperature 248 °F
1 mm/min; ISO 527
3.25 GPa

@Temperature 80.0 °C
471 ksi

@Temperature 176 °F
1 mm/min; ISO 527
Flexural Modulus 3.90 GPa
566 ksi
2 mm/min, 64mm span; ISO 178
2.85 GPa

@Temperature 80.0 °C
413 ksi

@Temperature 176 °F
2 mm/min, 64mm span; ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4mm, Cut; ISO 180/1A
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
80*10*4mm, Cut; ISO 179/1eA
1.80 J/cm²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
80*10*4mm, Cut; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 156 °C
313 °F
80*10*4mm, Cut; ISO 75-1&2
Users viewing this material also viewed the following: