Material Notes:
SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ISO 868
Tensile Strength at Break 18.0 MPa
2610 psi
Type I, 50 mm/min; ASTM D638
29.0 MPa
4210 psi
50 mm/min, 1A; ISO 527
Tensile Strength, Yield 35.0 MPa
5080 psi
Type I, 50 mm/min; ASTM D638
37.0 MPa
5370 psi
50 mm/min; ISO 527
Elongation at Break 25.6 %
25.6 %
Type I, 50 mm/min; ASTM D638
50 %
50 %
50 mm/min; ISO 527
Elongation at Yield 4.9 %
4.9 %
50 mm/min; ISO 527
5.5 %
5.5 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.71 GPa
393 ksi
50 mm/min; ASTM D638
3.10 GPa
450 ksi
1 mm/min; ISO 527
Flexural Modulus 2.70 GPa
392 ksi
1.3 mm/min, 50 mm span; ASTM D790
3.14 GPa
455 ksi
2 mm/min, 64mm span; ISO 178
Izod Impact, Notched 0.210 J/cm
0.393 ft-lb/in
63.5*12.7*3.2mm, Cut; ASTM D256
Izod Impact, Unnotched 4.49 J/cm
8.41 ft-lb/in
63.5*12.7*3.2mm, Cut; ASTM D4812
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4mm, Cut; ISO 180/1A
1.00 kJ/m²

@Temperature -30.0 °C
0.476 ft-lb/in²

@Temperature -22.0 °F
80*10*4mm, Cut; ISO 180/1A
2.00 kJ/m²

@Temperature 0.000 °C
0.952 ft-lb/in²

@Temperature 32.0 °F
80*10*4mm, Cut; ISO 180/1A
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
80*10*4mm, Cut; ISO 179/1eA
0.100 J/cm²

@Temperature -30.0 °C
0.476 ft-lb/in²

@Temperature -22.0 °F
80*10*4mm, Cut; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature -30.0 - 100 °C
38.9 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature -30.0 - 100 °C
65.0 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
80*10*4mm, Cut; ISO 75-1&2
125 °C

@Thickness 3.20 mm
257 °F

@Thickness 0.126 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
163 °F
80*10*4mm, Cut; ISO 75-1&2
68.0 °C

@Thickness 3.20 mm
154 °F

@Thickness 0.126 in
ASTM D648
Vicat Softening Point 150 °C
302 °F
10N, 50°C/hr; ISO 306