Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl PKN4736 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+PS. FDA compliant. High heat. Excellent ESCR. Extrusion. Microwavable. Food packaging uses.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D 785
Tensile Strength at Break 55.0 MPa
7980 psi
Type I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 64.0 MPa
9280 psi
Type I, 50 mm/min; ASTM D 638
Elongation at Break 28 %
28 %
Type I, 50 mm/min; ASTM D 638
Elongation at Yield 9.5 %
9.5 %
Type I, 50 mm/min; ASTM D 638
Flexural Yield Strength 99.0 MPa
14400 psi
2.6 mm/min, 100 mm span; ASTM D 790
Flexural Modulus 2.28 GPa
331 ksi
2.6 mm/min, 100 mm span; ASTM D 790
Izod Impact, Notched 0.960 J/cm

@Temperature 23.0 °C
1.80 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C

@Thickness 6.40 mm
289 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C

@Thickness 6.40 mm
264 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Vicat Softening Point 155 °C
311 °F
Rate B/50; ASTM D 1525