SABIC Innovative Plastics Noryl PKN4717 PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl PKN4717 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+PS. Translucent. FDA compliant. High heat. Foam extrusion. Microwavable. Food packaging uses. Solid properties listed.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D 792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D 570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124
124
ASTM D 785
Tensile Strength at Break 83.0 MPa
12000 psi
Type I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 83.0 MPa
12000 psi
Type I, 50 mm/min; ASTM D 638
Elongation at Break 93 %
93 %
Type I, 50 mm/min; ASTM D 638
Elongation at Yield 9.1 %
9.1 %
Type I, 50 mm/min; ASTM D 638
Flexural Yield Strength 128 MPa
18600 psi
2.6 mm/min, 100 mm span; ASTM D 790
Flexural Modulus 3.03 GPa
439 ksi
2.6 mm/min, 100 mm span; ASTM D 790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C

@Thickness 6.40 mm
289 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C

@Thickness 6.40 mm
270 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Vicat Softening Point 157 °C
315 °F
Rate B/50; ASTM D 1525