Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Noryl GFN2L PPE+HIPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) , Polystyrene + Polyphenylene Ether, Unreinforced , Polystyrene, Impact Modified
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl GFN2L PPE+HIPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D 792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124
124
ASTM D 785
Tensile Strength, Yield 98.0 MPa
14200 psi
SABIC - Japan Method
Elongation at Break 4.0 - 6.0 %
4.0 - 6.0 %
SABIC - Japan Method
Flexural Strength 131 MPa
19000 psi
ASTM D 790
Flexural Modulus 5.57 GPa
808 ksi
ASTM D 790
Izod Impact, Notched 0.880 J/cm

@Temperature 23.0 °C
1.65 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 28.0 - 45.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.6 - 25.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 138 °C

@Thickness 3.20 mm
280 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D 257
Dielectric Constant 2.86

@Frequency 50.0 - 60.0 Hz
2.86

@Frequency 50.0 - 60.0 Hz
ASTM D 150
Arc Resistance 60 - 120 sec
60 - 120 sec
Tungsten, PLC code 6; ASTM D 495
Copyright © lookpolymers.com All Rights Reserved