Material Notes:
High gloss, general purpose grade. 130C (266F) DTUL. UL 94 HB rated. For multiple plugs, wine filter plates, etc.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D 792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D 785
Tensile Strength, Yield 66.0 MPa
9570 psi
Type I, 50 mm/min; ASTM D 638
Flexural Yield Strength 93.0 MPa
13500 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.48 GPa
360 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 1.33 J/cm

@Temperature -40.0 °C
2.49 ft-lb/in

@Temperature -40.0 °F
ASTM D 256
2.67 J/cm

@Temperature 23.0 °C
5.00 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Gardner Impact 5.00 J

@Temperature -40.0 °C
3.69 ft-lb

@Temperature -40.0 °F
ASTM D 3029
25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
ASTM D 3029
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 59.4 µm/m-°C

@Temperature -40.0 - 95.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 137 °C

@Thickness 6.40 mm
279 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C

@Thickness 6.40 mm
264 °F

@Thickness 0.252 in
unannealed; ASTM D 648
UL RTI, Electrical 105 °C
221 °F
UL 746B
UL RTI, Mechanical with Impact 90.0 °C
194 °F
UL 746B
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
UL 94
Electrical Properties Metric English Comments
Dielectric Constant 2.65

@Frequency 50.0 - 60.0 Hz
2.65

@Frequency 50.0 - 60.0 Hz
ASTM D 150
Dielectric Strength 21.6 kV/mm

@Thickness 3.20 mm
549 kV/in

@Thickness 0.126 in
in oil; ASTM D 149
Dissipation Factor 0.00040

@Frequency 50.0 - 60.0 Hz
0.00040

@Frequency 50.0 - 60.0 Hz
ASTM D 150
Arc Resistance 0.00 - 60 sec
0.00 - 60 sec
Tungsten, PLC code 7; ASTM D 495
Comparative Tracking Index 175 - 250 V
175 - 250 V
PLC code 3; UL 746A
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
PLC code 2; UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
surface, PLC code 0; UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
>= 5.91 in/min
PLC code 4; UL 746A