SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 50265-2-1 requirement. 93 Shore A hardness. Processing typically conducted on standard extrusion equipment. Wire tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Melt Flow 8.5 g/10 min

@Load 10.0 kg,
Temperature 250 °C
8.5 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
30S reading; ASTM D2240
Tensile Strength at Break 9.00 MPa
1310 psi
Type I, 50 mm/min; ASTM D638
9.00 MPa
1310 psi
50 mm/min; ISO 527
15.0 MPa
2180 psi
UL 1581
15.0 MPa
2180 psi
after 7days @80°C; UL 1581
Elongation at Break 130 %
130 %
Type I, 50 mm/min; ASTM D638
175 %
175 %
50 mm/min; ISO 527
267 %
267 %
after 7days @136°C; UL 1581
306 %
306 %
UL 1581
Flexural Modulus 0.130 GPa
18.9 ksi
12.5 mm/min; ISO 178
0.160 GPa
23.2 ksi
12.5 mm/min, 100 mm span; ASTM D790
Heat Distortion 10 %

@Load 0.250 kg,
Temperature 100 °C
10 %

@Load 0.551 lb,
Temperature 212 °F
UL 1581
Thermal Properties Metric English Comments
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Oxygen Index 29 %
29 %
ISO 4589
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
750 °C

@Thickness 3.00 mm
1380 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 22.9 kV/mm

@Thickness 2.00 mm
582 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0010

@Frequency 1.00e+6 Hz
0.0010

@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 56
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 152
ASTM E 662
Vertical Flame Test PASSES
EN 50265-2-1