Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL SE100V PPE+HIPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL SE100V PPE+HIPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 43.0 MPa
6240 psi
SABIC - Japan Method
Elongation at Break 55 %
55 %
SABIC - Japan Method
Flexural Strength 71.0 MPa
10300 psi
ASTM D790
Flexural Modulus 2.25 GPa
326 ksi
ASTM D790
Izod Impact, Notched 2.54 J/cm
4.76 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 100 °C

@Thickness 3.20 mm
212 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 0.710 mm
HB

@Thickness 0.0280 in
UL 94
V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94
5VB

@Thickness 2.80 mm
5VB

@Thickness 0.110 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Dielectric Constant 2.65

@Frequency 50.0 - 60.0 Hz
2.65

@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 60 - 120 sec
60 - 120 sec
Tungsten; ASTM D495