SABIC Innovative Plastics NORYL PX2622 PPE+HIPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PX2622 PPE+HIPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE/HIPS for auto interior
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.20 mm
0.0060 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 12.1 g/10 min

@Load 10.0 kg,
Temperature 250 °C
12.1 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
SABIC - Japan Method
Elongation at Break 50 %
50 %
SABIC - Japan Method
Flexural Strength 73.0 MPa
10600 psi
ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
33.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 120 °C

@Thickness 6.40 mm
248 °F

@Thickness 0.252 in
unannealed; ASTM D648