Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PCN2615 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Melt Flow 14 g/10 min

@Load 5.00 kg,
Temperature 300 °C
14 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 116 MPa
16800 psi
Type I, 10 mm/min; SABIC - Japan Method
Elongation at Yield 7.0 %
7.0 %
Type I, 10 mm/min; SABIC - Japan Method
Flexural Yield Strength 160 MPa
23200 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 8.30 GPa
1200 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.780 J/cm
1.46 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 125 °C

@Thickness 6.40 mm
257 °F

@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94 V-1

@Thickness 2.00 mm
V-1

@Thickness 0.0787 in
UL 94