Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of strength and dimensional stability. This grade can be processed via extrusion or injection molding. Noryl NH7114 is available in custom colors and may be an excellent material candidate for use in electrical and electronics markets.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Moisture Absorption 0.0700 %
0.0700 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.22 %
0.22 %
ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0030 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 5.8 g/10 min

@Load 5.00 kg,
Temperature 280 °C
5.8 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 300 °C
10 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 105 MPa
15200 psi
5 mm/min; ISO 527
107 MPa
15500 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 105 MPa
15200 psi
5 mm/min; ISO 527
107 MPa
15500 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 2.0 %
2.0 %
Type I, 5 mm/min; ASTM D638
2.0 %
2.0 %
5 mm/min; ISO 527
Elongation at Yield 2.0 %
2.0 %
Type I, 5 mm/min; ASTM D638
2.0 %
2.0 %
5 mm/min; ISO 527
Tensile Modulus 6.80 GPa
986 ksi
5 mm/min; ASTM D638
6.80 GPa
986 ksi
1 mm/min; ISO 527
Flexural Yield Strength 150 MPa
21800 psi
2 mm/min; ISO 178
152 MPa
22000 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6.00 GPa
870 ksi
1.3 mm/min, 50 mm span; ASTM D790
6.30 GPa
914 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.770 J/cm
1.44 ft-lb/in
ASTM D256
0.700 J/cm

@Temperature -30.0 °C
1.31 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
6.00 kJ/m²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
80*10*4; ISO 180/1U
27.0 kJ/m²

@Temperature -30.0 °C
12.8 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
3.00 J/cm²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 15.0 J

@Temperature 23.0 °C
11.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 51.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
51.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 68.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
68.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
140 °C

@Thickness 3.20 mm
284 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 148 °C
298 °F
Rate B/50; ASTM D1525
148 °C
298 °F
Rate B/50; ISO 306
150 °C
302 °F
Rate B/120; ISO 306
UL RTI, Electrical 110 °C
230 °F
UL 746B
UL RTI, Mechanical with Impact 105 °C
221 °F
UL 746B
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94 by SABIC-IP
V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
UL 94 by SABIC-IP
5VA

@Thickness 2.00 mm
5VA

@Thickness 0.0787 in
UL 94 by SABIC-IP
Oxygen Index 30 %
30 %
ISO 4589
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
800 °C
1470 °F
IEC 60695-2-13
960 °C

@Thickness 1.00 mm
1760 °F

@Thickness 0.0394 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 5.00e+17 ohm
>= 5.00e+17 ohm
ROA; IEC 60093
Dielectric Constant 2.7

@Frequency 1.00e+6 Hz
2.7

@Frequency 1.00e+6 Hz
IEC 60250
2.73

@Frequency 1.00e+6 Hz
2.73

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm

@Thickness 3.20 mm
406 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
25.0 kV/mm

@Thickness 3.20 mm
635 kV/in

@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor 0.0029

@Frequency 1.00e+6 Hz
0.0029

@Frequency 1.00e+6 Hz
ASTM D150
0.0029

@Frequency 1.00e+6 Hz
0.0029

@Frequency 1.00e+6 Hz
IEC 60250
Arc Resistance 180 - 240 sec
180 - 240 sec
UL 746A
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
0.00 - 15 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
>= 5.91 in/min
UL 746A
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2
Users viewing this material also viewed the following: