SABIC Innovative Plastics NORYL N190 PPE+HIPS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL N190 PPE+HIPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NORYL N190 is an unfilled, flame retardant material with a Vicat B/120 of 105°C according ISO 306. NORYL N190 is V0 at 1.52 mm and 5VA at 3.12 mm according UL94 and halogen free according VDE/DIN 472 part 815. NORYL N190 is available in all colours.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Moisture Absorption 0.0600 %
0.0600 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.32 %
0.32 %
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
on Tensile Bar; SABIC Method
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 280 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 87.0 MPa
12600 psi
ISO 2039-1
Tensile Strength at Break 40.0 MPa
5800 psi
50 mm/min; ISO 527
Tensile Strength, Yield 50.0 MPa
7250 psi
50 mm/min; ISO 527
Elongation at Break 20 %
20 %
50 mm/min; ISO 527
Elongation at Yield 3.0 %
3.0 %
50 mm/min; ISO 527
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min; ISO 527
Flexural Yield Strength 75.0 MPa
10900 psi
2 mm/min; ISO 178
Flexural Modulus 2.20 GPa
319 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
6.00 kJ/m²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ISO 8302
Hot Ball Pressure Test <= 95.0 °C
<= 203 °F
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 95.0 °C
203 °F
Rate B/50; ISO 306
105 °C
221 °F
Rate B/120; ISO 306
110 °C
230 °F
Rate A/50; ISO 306
UL RTI, Electrical 95.0 °C
203 °F
UL 746B
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
UL RTI, Mechanical without Impact 95.0 °C
203 °F
UL 746B
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in
UL 94
Oxygen Index 30 %
30 %
ISO 4589
Glow Wire Test 960 °C

@Thickness 3.20 mm
1760 °F

@Thickness 0.126 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
IEC 60250
2.7

@Frequency 50.0 - 60.0 Hz
2.7

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dissipation Factor 0.00040

@Frequency 50.0 - 60.0 Hz
0.00040

@Frequency 50.0 - 60.0 Hz
IEC 60250
0.00090

@Frequency 1.00e+6 Hz
0.00090

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 250 V
250 V
IEC 60112
Descriptive Properties Value Comments
Ball Pressure Test, 75°C +/- 2°C PASSES
IEC 60695-10-2