Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL N110HG PPE+HIPS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL N110HG PPE+HIPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NORYL N110HG is an unfilled material, with a Vicat B/120 of 116°C according ISO 306. NORYL N110HG can be used in applications where high gloss is required.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Moisture Absorption 0.0700 %
0.0700 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %
0.20 %
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
on Tensile Bar; SABIC Method
Melt Index of Compound 15 g/10 min

@Load 3.80 kg,
Temperature 280 °C
15 g/10 min

@Load 8.38 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 95.0 MPa
13800 psi
ISO 2039-1
Tensile Strength at Break 40.0 MPa
5800 psi
50 mm/min; ISO 527
Tensile Strength, Yield 45.0 MPa
6530 psi
50 mm/min; ISO 527
Elongation at Break 30 %
30 %
50 mm/min; ISO 527
Elongation at Yield 3.0 %
3.0 %
50 mm/min; ISO 527
Tensile Modulus 2.20 GPa
319 ksi
1 mm/min; ISO 527
Flexural Yield Strength 60.0 MPa
8700 psi
2 mm/min; ISO 178
Flexural Modulus 2.00 GPa
290 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 115 °C
239 °F
Rate B/50; ISO 306
115 °C
239 °F
Rate B/120; ISO 306
120 °C
248 °F
Rate A/50; ISO 306
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
UL 94
Oxygen Index 19 %
19 %
ISO 4589
Glow Wire Test 960 °C

@Thickness 3.20 mm
1760 °F

@Thickness 0.126 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
IEC 60250
2.6

@Frequency 50.0 - 60.0 Hz
2.6

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor 0.0010

@Frequency 1.00e+6 Hz
0.0010

@Frequency 1.00e+6 Hz
IEC 60250
0.0040

@Frequency 50.0 - 60.0 Hz
0.0040

@Frequency 50.0 - 60.0 Hz
IEC 60250
Descriptive Properties Value Comments
Ball Pressure Test, 75°C +/- 2°C PASSES
IEC 60695-10-2
Users viewing this material also viewed the following: