SABIC Innovative Plastics NORYL GN390 PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GN390 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Closed loop recycle grade for CANON, 13% PCR-PS loaded, HDT 90C, V-0/1.2mm
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 28 g/10 min

@Load 10.0 kg,
Temperature 250 °C
28 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.0 MPa
9140 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 40 %
40 %
Type I, 50 mm/min; ASTM D638
Flexural Strength 85.0 MPa
12300 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 0.880 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C

@Thickness 6.40 mm
194 °F

@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C
176 °F
UL 746B
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
UL RTI, Mechanical without Impact 80.0 °C
176 °F
UL 746B
Flammability, UL94 V-0

@Thickness 1.20 mm
V-0

@Thickness 0.0472 in
UL 94
5VB

@Thickness 2.00 mm
5VB

@Thickness 0.0787 in
UL 94