Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 in limited colours.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Moisture Absorption 0.0600 %
0.0600 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %
0.20 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
on Tensile Bar; SABIC Method
Melt Index of Compound 7.0 g/10 min

@Load 10.0 kg,
Temperature 280 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 130 MPa
18900 psi
ISO 2039-1
Tensile Strength at Break 100 MPa
14500 psi
5 mm/min; ISO 527
Elongation at Break 1.5 %
1.5 %
5 mm/min; ISO 527
Tensile Modulus 8.00 GPa
1160 ksi
1 mm/min; ISO 527
Flexural Strength 125 MPa
18100 psi
2 mm/min; ISO 178
Flexural Modulus 6.00 GPa
870 ksi
2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
25.0 kJ/m²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Taber Abrasion, mg/1000 Cycles 70
70
CS-17, 1 kg; SABIC Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
16.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 145 °C
293 °F
Rate B/50; ISO 306
155 °C
311 °F
Rate B/120; ISO 306
155 °C
311 °F
Rate A/50; ISO 306
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical with Impact 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical without Impact 50.0 °C
122 °F
UL 746B
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94
Oxygen Index 26 %
26 %
ISO 4589
Glow Wire Test 850 °C

@Thickness 3.20 mm
1560 °F

@Thickness 0.126 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 2.9

@Frequency 1.00e+6 Hz
2.9

@Frequency 1.00e+6 Hz
IEC 60250
2.9

@Frequency 50.0 - 60.0 Hz
2.9

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm

@Thickness 3.20 mm
457 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor 0.00060

@Frequency 50.0 - 60.0 Hz
0.00060

@Frequency 50.0 - 60.0 Hz
IEC 60250
0.0010

@Frequency 1.00e+6 Hz
0.0010

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 250 V
250 V
IEC 60112
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2