SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating at 1.5 mm and a UL94 V0 rating at 3.0 mm. Noryl ENV131 is also halogen free according to VDE/DIN 472 part 815 and may be an excellent material candidate for extrusion moulded application where flame resistance and high temperature resistance is required. This Resin pass the BPT @ 125 deg C and has CTI > 450V in selected colors.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Moisture Absorption 0.0800 %
0.0800 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.29 %
0.29 %
ISO 62
Melt Index of Compound 11 g/10 min

@Load 10.0 kg,
Temperature 280 °C
11 g/10 min

@Load 22.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
50 mm/min; ISO 527
Tensile Strength, Yield 67.0 MPa
9720 psi
50 mm/min; ISO 527
Elongation at Break 9.0 %
9.0 %
50 mm/min; ISO 527
Elongation at Yield 4.0 %
4.0 %
50 mm/min; ISO 527
Tensile Modulus 2.45 GPa
355 ksi
1 mm/min; ISO 527
Flexural Yield Strength 100 MPa
14500 psi
2 mm/min; ISO 178
Flexural Modulus 2.49 GPa
361 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
9.00 kJ/m²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 79.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
79.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 82.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
234 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 132 °C
270 °F
Rate B/50; ISO 306
138 °C
280 °F
Rate B/120; ISO 306
UL RTI, Electrical 65.0 °C
149 °F
UL 746B
UL RTI, Mechanical with Impact 65.0 °C
149 °F
UL 746B
UL RTI, Mechanical without Impact 65.0 °C
149 °F
UL 746B
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
UL 94
Glow Wire Test 960 °C

@Thickness 1.00 mm
1760 °F

@Thickness 0.0394 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.17e+16 ohm-cm
1.17e+16 ohm-cm
ASTM D257
Surface Resistance 8.95e+13 ohm
8.95e+13 ohm
ASTM D257
Dielectric Constant 2.8

@Frequency 1.00e+6 Hz
2.8

@Frequency 1.00e+6 Hz
ASTM D150
2.8

@Frequency 1.00e+6 Hz
2.8

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 24.5 kV/mm

@Thickness 1.60 mm
622 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
Comparative Tracking Index 450 V
450 V
IEC 60112
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2