SABIC Innovative Plastics NORYL 844 PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL 844 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium heat PPO/HIPS alloy used in the automotive industry.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.0 MPa
5660 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 41 %
41 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 68.0 MPa
9860 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.97 J/cm
3.69 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C

@Thickness 3.20 mm
205 °F

@Thickness 0.126 in
unannealed; ASTM D648
108 °C

@Thickness 6.40 mm
226 °F

@Thickness 0.252 in
unannealed; ASTM D648