Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Lexan® ML7667 PC Copolymer

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® ML7667 PC Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.0mm flame retardancy based on non-chlorine, non-bromine FR agents with excellent processability, improved release performance and good impact performance. This product is available in limited opaque colors only and may be an excellent candidate for a broad range of applications, i.e. electrical and electronic enclosure applications.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
Moisture Absorption 0.400 %
0.400 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.15 %
0.15 %
ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Melt Index of Compound 8.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
8.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
Type I, 5 mm/min; ASTM D638
46.0 MPa
6670 psi
5 mm/min; ISO 527
Tensile Strength, Yield 54.0 MPa
7830 psi
5 mm/min; ISO 527
55.0 MPa
7980 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 13 %
13 %
5 mm/min; ISO 527
15 %
15 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 4.4 %
4.4 %
Type I, 5 mm/min; ASTM D638
4.4 %
4.4 %
5 mm/min; ISO 527
Tensile Modulus 3.50 GPa
508 ksi
5 mm/min; ASTM D638
3.60 GPa
522 ksi
1 mm/min; ISO 527
Flexural Yield Strength 96.0 MPa
13900 psi
2 mm/min; ISO 178
97.0 MPa
14100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.15 GPa
457 ksi
1.3 mm/min, 50 mm span; ASTM D790
3.40 GPa
493 ksi
2 mm/min; ISO 178
Izod Impact, Notched 3.40 J/cm
6.37 ft-lb/in
ASTM D256
1.50 J/cm

@Temperature -30.0 °C
2.81 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*3; ISO 180/1A
10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*3; ISO 180/1U
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NB
NB
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 2.50 J/cm²
11.9 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
1.50 J/cm²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 47.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
47.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
70.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
135 °C

@Thickness 3.20 mm
275 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 145 °C
293 °F
Rate B/50; ISO 306
146 °C
295 °F
Rate B/120; ISO 306
146 °C
295 °F
Rate B/50; ASTM D1525
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
UL 94 by SABIC-IP
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94 by SABIC-IP
5VB

@Thickness 3.00 mm
5VB

@Thickness 0.118 in
UL 94 by SABIC-IP
Glow Wire Test 825 °C
1520 °F
IEC 60695-2-13
825 °C
1520 °F
IEC 60695-2-13
825 °C
1520 °F
IEC 60695-2-13
825 °C
1520 °F
IEC 60695-2-13
960 °C

@Thickness 1.10 mm
1760 °F

@Thickness 0.0433 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Comparative Tracking Index 175 V
175 V
IEC 60112
175 - 250 V
175 - 250 V
UL 746A
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C passes
IEC 60695-10-2