Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Lexan® LCG2007 PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® LCG2007 PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Water Absorption 0.12 %

@Time 86400 sec
0.12 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0015 - 0.0025 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0025 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell M 94
94
ASTM D785
Tensile Strength, Yield 132 MPa
19100 psi
SABIC - Japan Method
Elongation at Break 5.0 - 7.0 %
5.0 - 7.0 %
SABIC - Japan Method
Flexural Strength 217 MPa
31500 psi
ASTM D790
Flexural Modulus 14.9 GPa
2160 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 20.0 - 45.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.1 - 25.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 138 °C

@Thickness 3.20 mm
280 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D257
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved