Material Notes:
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). Contains a higher amount of mold release than HPS6.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.15 %

@Time 86400 sec
0.15 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength at Break 68.0 MPa
9860 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa
8990 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 135 %
135 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 97.0 MPa
14100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 9.07 J/cm
17.0 ft-lb/in
ASTM D256
Izod Impact, Unnotched 32.04 J/cm
60.02 ft-lb/in
ASTM D4812
Dart Drop, Total Energy 64.0 J
47.2 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 137 °C

@Thickness 6.40 mm
279 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C

@Thickness 6.40 mm
270 °F

@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 154 °C
309 °F
Rate B/50; ASTM D1525