Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON RV00CEXP PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RV00CEXP PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* RV00CE is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ISO 1183
Water Absorption 0.90 %

@Time 86400 sec
0.90 %

@Time 24.0 hour
ISO 62-1
Moisture Absorption 1.10 %
1.10 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0026 cm/cm
0.0026 in/in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0061 cm/cm
0.0061 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 270 MPa
39200 psi
5 mm/min; ISO 527
Elongation at Break 1.7 %
1.7 %
5 mm/min; ISO 527
2.6 %
2.6 %
Flexural Strain, break, 2 mm/min; ISO 178
Tensile Modulus 21.6 GPa
3130 ksi
1 mm/min; ISO 527
Flexural Strength 430 MPa
62400 psi
2 mm/min; ISO 178
Flexural Modulus 19.0 GPa
2760 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 53.0 kJ/m²
25.2 ft-lb/in²
80*10*4; ISO 180/1A
43.0 kJ/m²

@Temperature -40.0 °C
20.5 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
9.44 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
29.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 255 °C
491 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
UL 94