Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON RV00AEX5 PA6.6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RV00AEX5 PA6.6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* Is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Water Absorption 0.90 %

@Time 86400 sec
0.90 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Time 86400 sec
0.0080 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 276 MPa
40000 psi
5 mm/min; ISO 527
Tensile Strength, Yield 276 MPa
40000 psi
5 mm/min; ISO 527
Elongation at Break 2.0 %
2.0 %
5 mm/min; ISO 527
Elongation at Yield 2.0 %
2.0 %
5 mm/min; ISO 527
Tensile Modulus 17.8 GPa
2580 ksi
1 mm/min; ISO 527
Flexural Yield Strength 366 MPa
53100 psi
2 mm/min; ISO 178
Flexural Modulus 15.0 GPa
2180 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 90.0 kJ/m²
42.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 259 °C
498 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 256 °C
493 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
UL RTI, Electrical 105 °C
221 °F
UL 746B
UL RTI, Mechanical with Impact 110 °C
230 °F
UL 746B
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
UL 94
Users viewing this material also viewed the following: