Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON PX91200 PA 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON PX91200 PA 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP VERTON* PX91200 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added features of this material include: High Impact, Structural
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 181 MPa
26300 psi
ISO 527
Elongation at Break 2.0 %
2.0 %
ISO 527
Tensile Modulus 12.1 GPa
1750 ksi
1 mm/min; ISO 527
Flexural Strength 250 MPa
36300 psi
ISO 178
Flexural Modulus 10.29 GPa
1492 ksi
ISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 222 °C
432 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Copyright © lookpolymers.com All Rights Reserved