SABIC Innovative Plastics LNP Thermotuf R1000IX2 PA6.6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermotuf R1000IX2 PA6.6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOTUF* R1000IX2 is a compound based on PA 66 resin, containing Impact Modifier. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.010 - 0.015 cm/cm
0.010 - 0.015 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
50 mm/min; ISO 527
Elongation at Break >= 40 %
>= 40 %
50 mm/min; ISO 527
Tensile Modulus 2.20 GPa
319 ksi
1 mm/min; ISO 527
Flexural Yield Strength 70.0 MPa
10200 psi
2 mm/min; ISO 178
Flexural Modulus 2.00 GPa
290 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af